Abstract:Polyacrylonitrile(PAN) stabilization fibers and carbon fibers were prepare from PAN precursors.Effect of thermal treating time at 250 ℃ of PAN fibers on their evolution to carbon fibers was investigated by Fourier transform infrared spectroscopy(FT-IR),element analysis(EA),wide-angle X-ray diffraction(WAXD) and differential scanning caborimetry(DSC).Two kinds of PAN precursors with different chemical compositions were used for comparison.It is found that when thermal treating time at 250 ℃ is more than 9 min,the increasing rate of relative cyclization index(RCI),density and aromatization index(AI) of stabilization fibers become slow,carbon fibers with bigger d002 of crystallite and Vp of carbon fibers can be got,worse crystallite layers pile up,more microvoid content and less tensile strength appear.