Abstract:Polyacrylonitrile(PAN) precursor was an important material to produce carbon fiber,however,its microstructure,especially the defects,had a significant effect on the strength of carbon fiber.The precursor was processed in 0T,8T,12T,16T high magnetic fields.The effects of magnetic field on crystal orientation,total orientation,crystal size,crystallinity were studied.The results show that magnetic field can induce the orientation in both crystal and amorphous regions.The orientation increases as the magnetic field intensity strengthens and the same result could be obtained when the processing time extends.Magnetic field can promote the conversion from the amorphous region to the crystal region,resulting at an increase of crystal size,crystallinity and density.Therefore,defects of fiber decreases and the strength of fibers increases.