Abstract:Polyether-polyol modified montmorilonites (POP-OMMT) were prepared using organo-montmorilonites (OMMT) as raw material. XRD analysis suggests that the oligomer polyether polyols intercalated into the inter layers of the organo montmoriased by 22.50 kPa, 35.35 kPa and 28.15% respectively,the initial decomposition temperature increased by 3.62 ℃. The tests show that mechanical properties and thermal stability of the nanocomposites are better than those of pure PU. lonites, and enlarged the basal spacing of the modified clays from 2.1 nm to 3.9 nm. Rigid polyurethane foam nanocomposites were synthesized by the reaction of POP-OMMT with polymethylidyne polyphenyl polyisocyanate, polyether polyols, chain extender, crosslinking agent and accessory ingredients. When 3.50%POP-MMT was added to PU, the compressions strength, bend strength and extension increased by 22.50kPa,35.35kPa and 28.15% respectively,the initialde composition temperature increased by 3.62℃.The tests show that mechanical properties and thermal stability of the nanocomposites are better than those of pure PU.