Abstract:Zinc aluminate was synthesized by sol gel method. The influences H2SO4, charge ratio of metal ion(Zn2+, Al3+), ethylene glycol and chelating agent (R) and calcining heat were discussed and characterized through X-ray diffraction (XRD) and scanning electron microscopy (SEM). At the condition such as H2SO4 in the system, the precursor heat treated at 700 ℃ in air for 2 h, R of 1∶2∶6∶30, high purity of ZnAl2O4 was obtained. Added ZnAl2O4 and the mixture of ZnAl2O4 and Sb2O3 in the flexible PVC, experiment results show when 1phr ZnAl2O4 was used, PVC show the excellent flame retardant and smoke suppression, limiting oxygen index (LOI) is 28.8%, smoke density rating (SDR) is 75.68%. When 10phr ZnAl2O4 and Sb2O3 mixture with the corresponding mass ratio of 2∶8 was used, a much better flame retardant was got, LOI of 35.8%, SDR of 92.16%.