Amino-terminal nylon-6 prepolymer with average molecular weight about 1000 (PA1000) and isocyanate-terminal polyether prepolymer (OPU) were synthesized respectively, and then the thermoplastic elastomer (TPE) based on nylon-6 was synthesized with the reaction between PA1000 and OPU in dimethyl acetamide (DMAC). The structure and properties of the synthesized TPE were studied by FT-IR, WAXD, DSC, TG, POM, stress-strain curves and dissolved test. The results show that the synthesized TPE exhibits a similar stress-strain behavior as crosslinked rubber, and has a high tensile strength and high elongation at break. TPE can be possessed of both high melt temperature (>170 ℃) and low glass transition temperature (<-80 ℃) together. It also has a good resistance to a lot of common solvents like pure nylon polymer and a good thermal stability. A new TPE with excellent comprehensive properties has been developed.
参考文献
相似文献
引证文献
引用本文
雷景新,郭东阳,高 峻,周昌林.聚酰胺弹性体的合成及结构与性能分析[J].高分子材料科学与工程,2014,30(2):100-104. Jingxin Lei, Dongyang Guo, Jun Gao, Changlin Zhou. Synthesis, Structure and Properties of Nylon Elastomer[J]. Polymer Materials Science & Engineering,2014,30(2):100-104.