Abstract:The aliphatic poly(ether-ester)s thermoplastic elastomers based on poly(butylene succinate) (PBS) as hard segment and poly(tetramethylene oxide) (PTMO, Mn=1000) as soft segment were synthesized. The mass fraction of soft PTMO segments in the polymer chains is 50%, 60% and 70%. The copolymers were characterized by 1H nuclear magnetic resonance spectrum (1H-NMR), permeation chromatography (GPC), differential scanning calorimetry (DSC) and mechanical test. Mn and Mw of the poly(ether-ester)s are higher than 5.0×104 and 13.0×104 respectively. Crystallization temperature (Tc) of PTMO soft blocks is -17.9 ℃,-14 ℃ and -17.4 ℃; however, that of PBS is 54.6 ℃ and 46.3 ℃. The deformation behavior of the synthesized poly(ether-ester)s shows the characteristics of thermoplastic elastomers. Stress at break of PBSPTMO50, PBSPTMO60 and PBSPTMO70 is approximately 22 MPa, 18 MPa and 14 MPa respectively. Elongation at break of all three samples reaches above 700%. The recovery rates tests show that the aliphatic poly(ether-ester)s thermoplastic elastomers have good recovery properties.