A series of block copolymers (PBS-PPS) were synthesized using poly 1, 3-propylene sebacate (PPS) as soft segment and butylene succinate (PBS) as hard segment through direct polymerization. The products were characterized by IR, 1H-NMR,DSC,GPC and SEM. The influence of monomer mass ratio on crystallinity, thermal properties and degradability of the copolymers was studied. The results show that the structure of the generated polymer is a typical polyester structure. With accumulation of PPS chain segment, the crystallinity of PBS is 68.00%, that of PBS-PPS10∶3 decreases to 35.5%. The mass loss rate of PBS is 27%, that of PBS-PPS10∶3 increase to 71% in enzyme solution after 10 weeks. Meanwhile, the decreasing degree of relative molecular mass is 35% for PBS and 81% for PBS-PPS10∶3. Damage of surface morphology and ester bond hydrolysis of the copolymer after degradation are significantly enhanced.
参考文献
相似文献
引证文献
引用本文
康宗华,王昌禄. BS-PPS生物降解聚酯的合成与降解性能[J].高分子材料科学与工程,2014,30(4):44-49. Zonghua Kang, Changlu Wang. Synthesis and Degradable Properties of Biodegradable PBS-PPS[J]. Polymer Materials Science & Engineering,2014,30(4):44-49.