    摘要:

    由聚乙二醇(PEG)、对苯二异氰酸酯(PPDI)、2,2-双(羟基甲基)丙酸(DMPA)和藻红B(EB)为主要原料,采用一步合成法合成了一系列带有自由羧基的荧光聚氨酯多嵌段共聚物。通过核磁共振氢谱、傅里叶变换红外光谱、凝胶渗透色谱法等测试方法表征了聚合物的结构。荧光光谱证实EB被成功地接在聚氨酯多嵌段共聚物上;动态激光光散射法测得该嵌段聚合物胶束粒径为208nm 左右;透射电子显微镜表明该胶束粒子呈现出球型形态。

    Abstract:

    A series of fluorescent poly(ethylene glycol) (PEG)-polyurethane multiblock copolymers with free carboxyl groups were synthesized by one-step method and their chemical structure and properties were investigated. PEG-polyurethane multiblock copolymers were composed of poly(ethylene glycol), 1,4-phenylene diisocyanate (PPDI), 2,2- bis(hydroxymethyl) propionic acid (DMPA) and fluorescent dye erythrosine B (EB). The structure of the resulting polymers was confirmed by 1H-NMR, FT-IR, gel permeation chromatography (GPC). The fluorescent spectra show that EB can be successfully conjugated onto PEG-polyurethane. The particle size of the block polymer micelle measured by the dynamic light scattering (DLS) is about 208 nm. The spherical micelle morphology of PEG-polyurethane copolymer was confirmed by TEM.

    参考文献
    相似文献
    引证文献
引用本文

金 晶,刘宇航,杨洪雨,张明耀.带有羧基基团荧光聚氨酯材料的合成与表征[J].高分子材料科学与工程,2014,30(5):11-15. Jing Jin, Yuhang Liu, Hongyu Yang, Mingyao Zhang. Synthesis and Characterization of Fluorescent Poly(Ethylene Glycol)-Polyurethane with Carboxyl Groups[J]. Polymer Materials Science & Engineering,2014,30(5):11-15.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2014-05-15
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司