Abstract:The granular poly(acrylic acid-sodium acrylate) bentonite composite was prepared by suspension polymerization with bentonite as main materials, a small amount of acrylic acid as polymeric monomer, Span80 as dispersant, cyclohexane as continuous phase, potassium persulfate as initiator, N,N-methylene-bis-acrylamide as cross linking agent. According to the dissolution quantity of acrylic acid and the adsorption capacity of Cd2+, the optimization experiment of the synthesis of granular poly(acrylic acid-sodium acrylate) bentonite was carried out. The optimized conditions are following: polymerization temperature is 70 ℃, polymerization time is 3h, the volume ratio of cyclohexane and span 80 is 52.5∶2.5, the oil/water ratio is 100∶15. The water phase is mixture of bentonite,acrylic acid, sodium hydroxide and water. Through the characterization of raw materials and products by X-ray diffraction(XRD), infrared spectrum analysis(IR) and scanning electron microscopy(SEM), the mechanism of copolymerization was discussed. The results indicate that acrylic acid and sodium acrylate are intercalated into the interlayer of bentonites and the polymerization carries out, which does not destroy the basic structure of bentonite. The sorption experiments of Pb2+, Cd2+and F- show that the adsorption capacity of composite bentonite is higher than that of Ca-bentonite.