改性魔芋葡甘聚糖/生物可降解聚酯静电纺丝
DOI:
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

基金项目:

四川省教育厅成果转化培育项目(12ZZ005);生物质材料教育部工程研究中心开放基金(13zxbk01)


Electrospinning of Thermoplastic Deacetylated Konjac Glucomannan /Biodegradable Polyesters
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为了制备改性魔芋葡甘聚糖(TDKGM)/生物可降解聚酯纳米复合纤维,以TDKGM和生物可降解聚酯(BP)为原料,三氟乙酸为溶剂,调节TDKGM和BP共混比例,采用静电纺丝方法分别制备了TDKGM/聚乳酸(PLA)、TDKGM/聚丁二酸丁二醇酯(PBS)纳米复合纤维。探讨了TDKGM与可降解聚酯共混比例对纺丝溶液的电导率、表面张力、流变性以及复合纤维直径、形貌和力学强度的影响。随着BP的增加,TDKGM/PLA共混液的表面张力从22.2 N/m降至18.2 N/m,电导率从69.7 μS/m 下降至39.1 μS/m;TDKGM/PBS共混液的表面张力从22.8 N/m降低到17.0 N/m;储能模量、损耗模量、剪切黏度都随之降低;而TDKGM/PBS共混液的电导率变化不成线性规律。当TDKGM/PLA比例为5∶5、TDKGM/PBS比例为6∶4时得到的纤维形貌最为理想,纳米复合纤维的直径分布在400~600 nm,100~500 nm范围,纤维膜的拉伸强度分别为3.557 MPa,4.543 MPa。TDKGM和BP共混比例将影响共混液的电导率、表面张力、流变性,从而影响静电纺丝复合纤维直径分布和形貌,通过控制TDKGM和BP共混比例可以成功地纺丝出纤维直径可控、强度高的TDKGM/BP纳米复合纤维。

    Abstract:

    The composite nanofibres of thermoplastic deacetylated konjac glucomannan (TDKGM)/ biodegradable polyesters (BP) were prepared by electricity spinning. TDKGM, polylactic acid (PLA) and poly butylene succinate (PBS) were, respectively, blended in the different mass ratio and dissolved in the trifluoroacetic acid (TFA). The effect of the blending ratio of TDKGM to BP on the surface tension, conductivity and rheological properties of the blending solution and the morphology, diameter and mechanical property of nanofibers were investigated. With increasing the BP content, the surface tension and conductivity of TDKGM/PLA sol decrease, respectively, from 22.2 N/m to 18.2 N/m and 69.7 μS/m to 39.1 μS/m, the surface tension of TDKGM/PBS sol also decreases from 22.8 N/m to 17.0 N/m, and storage modulus, loss modulus and shear viscosity decrease. But the conductivity of TDKGM/PBS sol is not changed linearly with increasing of the PBS content. When the mass ratio of TDKGM to PLA and PBS is 5∶5 and 6∶4, respectively, the composite nanofibers of TDKGM/BP can be fabricated with the fine morphology, diameter distribution of 400~600 nm and 100~500 nm and tensile strength of 3.557 MPa and 4.543 MPa respectively. The blending ratio of TDKGM/BP influences the surface tension, conductivity and rheological properties of the blending solution, further affects the diameter distribution of the composite nanofibers. The composite nanofibers of TDKGM/BP with the controllable fiber diameter and high-intensity can be fabricated via electrospinning by controlling the blending ratio of TDKGM to BP.

    参考文献
    相似文献
    引证文献
引用本文

杜欣辰, 林晓艳, 黄元昊, 李莹.改性魔芋葡甘聚糖/生物可降解聚酯静电纺丝[J].高分子材料科学与工程,2014,30(12):94-99. Xinchen Du, Xiaoyan Lin, Yuanhao Huang, Ying Li. Electrospinning of Thermoplastic Deacetylated Konjac Glucomannan /Biodegradable Polyesters[J]. Polymer Materials Science & Engineering,2014,30(12):94-99.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2014-12-12
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司