Synthesis of Two Disubstituted Monomers of Quinoxaline and Alternating Copolymerization with 2,5-Di Dodecyloxy-1,4-Diethynylbenzene and Optical Properties
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    以苯并噻二唑为初始原料,通过硝化、还原、缩合等反应合成了2种新型单体5,10-二溴-2,3,7,8-二萘基双喹喔啉(M1)和5,10-二溴-2,3,7,8-二菲基双喹喔啉(M2)。2种单体分别与1,4-二炔基-2,5-二氧十二烷基苯共聚,得到了2种新型共轭共聚物,聚(2,3,7,8-二萘基双喹喔啉-二炔基-2,5-二氧十二烷基苯)(P1)(产率86.1%)和聚(2,3,7,8-二菲基双喹喔啉-二炔基-2,5-二氧十二烷基苯)(P2)(产率41.6%)。所得单体通过红外光谱、核磁共振等进行了表征。单体和聚合物的紫外-可见吸收光谱中M1的最大吸收波长在339 nm,354 nm处出现。M2的最大吸收波长分别在304 nm, 317 nm处出现双吸收峰外,在长波431 nm,459 nm处出现双吸收峰。P1的最大吸收波长在448 nm处出现,在305 nm和317 nm 处出现2个吸收峰。P2在短波处吸收峰分别在350 nm,368 nm处出现。单体荧光光谱图中分别在 480 nm和579 nm出现最大发射峰。聚合物分别在487 nm和478 nm处出现最大发射峰。得到的共聚物通过X射线衍射发现结晶性较差。

    Abstract:

    Benzo-thiadiazole as primary material,5,10-dibromo-2,3,7,8-acenaphthene-quinoxaline (M1) and 5,10-dibromo-2,3,7,8-phenanthrene quinoxaline (M2) synthesized by nitration, reduction, and condensation reaction. Its alternating copolymers of poly(2,5-didodecyloxy-1,4-diethynyl-phenylene-alt-2,3,7,8-diacenaphthenequinoxaline)(P1) and poly(2,5-didodecyloxy-1,4-diethynyl-phenylene-alt-2,3,7,8-diphenanthrenequinoxaline)(P2) were prepared with 2,5-didodecyloxy-1,4-diethynlbenzene by Sonogashira reaction. And these structures of monomers were characterized by FT-IR and 1H-NMR. In the UV-Vis absorbance of the monomers and polymers, maximum absorption wavelength of M1 appears at 339 nm, 354 nm and 317 nm, 436 nm in CHCl3 respectively. The maximum absorption wavelength of the monomer M2 appears double absorption peaks at 304 nm, 317 nm; in long wave appear double absorption peaks at 431 nm, 459 nm. The maximum absorption wavelength of polymer P1 appears at 448 nm, two absorption peaks appear at 305 nm and 317 nm. The photoluminescence (PL) spectra of monomers show that that maximum emission peaks appear at 480 nm and 579 nm respectively, and the maximum emission peaks of polymers appear at 487 nm and 478 nm respectively. The XRD patterns of polymers obtained by X-ray diffraction (XRD) show lower crystallinity.

    参考文献
    相似文献
    引证文献
引用本文

阿卜杜合拜尔·米尔扎,司马义·努尔拉, 阿布都克尤木·阿布都热西提,古丽加娜提·排他尔, 买苏尔·米吉提, 吐尼莎古丽·阿吾提.萘基/菲基双取代喹喔啉单体衍生二炔基-烷氧基苯共聚[J].高分子材料科学与工程,2015,31(1):31-36. Abduheber Mirzehmet, Ismayil Nurulla, Abdukaiyum Abdurashid Guljannat Pattar, Maxur Mijit, Tunsagul Awut. Synthesis of Two Disubstituted Monomers of Quinoxaline and Alternating Copolymerization with 2,5-Di Dodecyloxy-1,4-Diethynylbenzene and Optical Properties[J]. Polymer Materials Science & Engineering,2015,31(1):31-36.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2015-02-01
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司