Abstract:Polylactide (PLLA)/polyvinyl alcohol (PVA) composites porous membranes were prepared by breath figure method. The effect of factors, such as composition of solvent, environmental humidity, polymer concentration, on the pores patterns and pore size was investigated. The results show that the solution is transparent using dimethylsulfoxide (DMSO)/DCM as blend solvent. PLLA/PVA composites honeycomb porous membranes with the diameter of (2.45±0.31) μm were prepared using DMSO/DCM=1/9(volume ratio of 1/9)as solvent. With increasing the DMSO content, the pore size is decreased and pore patterns become disorder. The pore size of PLLA/PVA composites porous membranes increases from (1.43±0.63) μm to (4.30±0.63) μm with increasing the environmental humidity from 43% to 91%. The relationship of pore size and the environmental humidity is presented first order liner relationship. Compared with pure PLLA porous membranes, the tensile strength and elongation at break of PLLA/PVA composites porous membranes increase from 33.32 MPa to 40.66 MPa and from 12.46% to 32.57%, respectively. These special PLLA/PVA membranes would be in favor of cell adhesion and growth, so they are expected to be very promising tissue engineering scaffold material.