Abstract:When glass fiber(GF) reinforced flame-retarded polyamide46 (GFFRPA46) was injection molding once, the recycled GFFRPA46 (RGFFRPA46) including the scraps and unqualified injection products was granulated by different extruders with varying screw configurations. GF of the RGFFRPA46 samples was observed by SEM and the size of more than 1000 GF were calculated. The average length (L) and the percentage of GF, of which the length is higher than the critical length (Vj), decrease with increase of the screw diameter and the length to diameter ratio (L/D). The extruded RGFFRPA46 prepared by a single screw extruder with 70 mm screw diameter and 4.3 L/D obtains the excellent mechanical properties, compared to those of RGFFRPA46, and the decrease ratio is lower than 3.6%. Moreover, its thermal properties are not significant different from those of RGFFRPA46. When RGFFRPA46 was extruded by a twin screw extruder, the L, the mechanical and thermal properties of the extruded RGFFRPA46 decrease significantly.