Abstract:Polylactide stereocomplex(sc-PLA) prepared by blending equivalent proportion of poly(L-lactic acid) /poly(D-lactic acid) (PLLA/PDLA) and its composites reinforced with 10% flax fibers were fabricated by melting compounding and followed by injection molding. Then the mechanical properties, crystallinity, cross-section morphology, and heat-resistance properties of two materials were studied by the mechanical property test, DSC, SEM, XRD, and Vicat softening point test. The results show that sc-PLA and 10% flax/sc-PLA composite exhibit both homocrystallites and stereocomplex crystallites. The crystallinity degree of composite is increased by reinforcement of flax fibers, and the yield of sc-crystallites of 10% flax/sc-PLA composite could reach 92.7%, higher than that of sc-PLA (66.4%). Compared with homopolymer PLLA, the heat-resistance property of sc-PLA is increased greatly, while its mechanical properties is decreased somewhat. By the addition of 10% flax fibers, the mechanical properties of sc-PLA are improved significantly, the tensile strength, elastic modulus and Izod notched impact strength of 10% flax/sc-PLA composite are increased by 34.1%, 49.8% and 289.1%, respectively. Moreover, 10% flax/sc-PLA composite shows a good heat-resistance property, and its Vicat softening temperature could achieve 155.6 ℃, increased nearly 92 ℃ than that of PLLA.