Abstract:PP precursor films with different contents of atactic polypropylene were prepared through casting process. After annealed under certain conditions, the precursor films were stretched uniaxially to develop micropores membranes. The oriented lamellar structure of the precursor was characterized by DSC, FT-IR, AFM and mechanical properties. The pore structure of the microporous membrane was characterized by porosity and permeability. The results show that small amount of a-PP in the precursor film could enhance moving ability of PP segment, and promote chain orientation along the drawing direction, giving rise to a more perfect oriented lamellar structure in the precursor films. However, more a-PP in the precursor will dilute the crystalline molecules, and promote segment relaxation, leading to decreased crystallinity and lamellar orientation in both crystalline and amorphous regions. Oriented lamellar structure of precursor films is further improved after annealing. The oriented lamellar structure in the precursor film that m(a-PP)/m(i-PP)=2/98 and is annealed at 120 ℃ is almost same perfect as in the precursor film that is without a-PP and is annealed at 145 ℃. The microporous membrane obtained by stretching precursor film with small amount of a-PP has a higher porosity and permeability. However, as a-PP content is increased in the precursor film, the porosity and permeability are decreased.