Abstract:The hydroxyl acrylic resin(PHA) was synthesized by solution polymerization, and the hydroxyl acrylic resin water dispersion was prepared by dispersing PHA in deionized water via emulsification process. By gel chromatography (GPC) tested the synthetic resin molecular weight, by rotary viscosimeter tested the viscosity, some through FT-IR characterization of the structure of the resin; the influence of polymer solution on molecular weight and water medium viscosity of the resin was studied, effects of cosolvent kind and amount on water medium viscosity were researched. The results show that with propylene glycol methyl ether acetate as solvent, two tertiary butyl peroxide as initiator at 120 ℃ in synthesis of PHA molecular weight minimum, when the dosage of solvent is 70%, hydroxyl acrylic resin with molecular weight of about 5000 can be obtained after 55% solvent is extracted at the end of polymerization;by emulsification method within the above PHA is dispersed in deionized water, when the solid content is 45%, the ethylene glycol butyl ether∶100# solvent oil is 1∶1 cosolvent to mix and dosage of cosolvent is 30%, the minimum water medium viscosity is 1000 mPa·s. Infrared spectrum analysis shows that goal polymer product is synthesized.