Abstract:Firstly the ultrasound was used to disperse the nano-Ag in production of porous polydimethylsiloxane (PDMS) membranes, with expectation of good bacteriostatic ability via dry-cast phase separation processing technique. The membrane morphologies were observed by digital microscopy. By choosing a suitable product formula, various performances of the porous PDMS with nano-Ag were tested. The results show that the average pore size of our products is as small as 2 μm. The mechanical property of the membrane drops along with increase of nano-Ag weight content. When only 0.0005% nano-Ag is added, the tensile strength for the membrane is 2.06 MPa, the elongation at break is 1278% and its elastic modulus is 0.22 MPa. Besides, the porous PDMS membrane with nano-Ag shows a better water vapor permeation ability than the IntegraTM artificial skin, the value reaching 163 g/(m2·24 h). The oxygen permeation ability of this membrane is also satisfactory, with an oxygen permeating coefficient as high as 2.87×10-8 (cm3·cm)/(cm2·s·Pa). Tests also prove that, as the nano-Ag has an observably bacteriostatic effect in addition to its safe release behavior, the membrane does not inhibit process of wound tissue rebuilding.