Abstract:To synthesize poly(3,4-ethylenedioxythiophene) (PEDOT) coating on polyethylene terephthalate(PET) film in situ and fabricate transparent conductive film, PET film was irradiated with 172 nm vacuum ultraviolet (VUV) to enhance the surface polarity and adsorption capacity, then dipped in Fe(OTs)3 solution to adsorb Fe(OTs)3 and finally suspended in EDOT solution to synthesize PEDOT coating in situ. The surface compositions of PET film after VUV irradiation were analyzed by ATR-FT-IR. The wetting ability of the irradiated surface was evaluated by water contacting angle and the adsorbing capacity to Fe(OTs)3 was determined by iodometry. The synthesized PEDOT coatings were identified through FT-IR and UV-vis spectroscope and the sheet resistance was measured by four point prob. The effect of VUV irradiating time on the transparency and conductivity of PEDOT/PET films was investigated. VUV irradiation introduces carboxylic groups to PET surface and improves the wettability and adsorption capacity of PET film. After irradiated for 4 min, the contacting angle decreases from 75° to 30° and the adsorbed Fe(OTs)3 amount increases from 0.9 mmol/m2 to 1.3 mmol/m2. As PET film with adsorbed Fe(OTs)3 is suspended in EDOT solution, the color of the film turns to pale blue gradually and becomes evener with VUV irradiation. FT-IR and UV-Vis spectra demonstrate that a positive charged PEDOT coating is hatched on PET film. Insulating PET film becomes conductive. At irradiating time of 4 min, the sheet resistance of the obtained PEDOT/PET film could be 900 Ω/□ and the transmittance is 80%.