Abstract:A series of sulfonated aromatic polyamides (SPA-50~SPA-70) containing fluorenyl and trifluoromethyl structures were successfully prepared by phosphorus acylation polycondensation using 9,9-bis(4-aminophenyl)fluorene-2,7-disulfonic acid with 1,4-bis(4-amino-2-trifluoromethyl-phenoxy) benzene and 4,4'- oxybisbenzoic acid. The structures of the sulfonated polymers were characterized by infrared spectroscopy (FT-IR) and nuclear magnetic resonance (NMR). The intrinsic viscosities of the sulfonated polymers are 0.80~0.94 dL/g, and the ion exchange capacity (IEC) values are 1.44~1.98 meq/g. All the sulfonated polymers have good solubility and film formation ability, and they could afford flexible and transparent membranes. Some properties, such as water uptake, swelling ratio, thermal and chemical stabilities and proton conductivity, were studied. The results indicate that SPA-70 (70% degree of sulfonation) has excellent combination properties: the water absorption is 23.5%, the swelling ratio is 8.6%, and the proton conductivity reaches 123 mS/cm at 80 ℃. Moreover, SPA-70 shows good chemical antioxidant stability and it could be retained for more than 6 h in Fenton solvents.