Abstract:To obtain highly improved mechanical properties, poly(ethylene-co-vinyl alcohol) (EVOH) was incorporated into poly(vinyl alcohol) (PVA) films by solution casting method. The surface and cross-section morphologies of all samples were characterized by scanning electron microscopy. FT-IR spectra show that the hydrogen bonds of PVA/EVOH blend films are gradually weakened with the increase of EVOH content. WAXD patterns indicate that the crystallinity of PVA/EVOH blend films is higher than that of pure PVA films, suggesting that the reduction of hydrogen bonds favors the alignment and arrangement of PVA macromolecules. Based on DSC curves, the endothermic peak temperature of PVA/EVOH blend film shifts to higher values, including the onset temperature and the end temperature. Moreover, mechanical properties of PVA/EVOH blend films depend on the content of EVOH. The maximum tensile strength, Young′s modulus and fracture energy of blend films could respectively reach 35.36 MPa, 3.87 N/mm and 0.032 J, which increase by 74.4%, 73.5% and 540% compared with those of pure poly(vinyl alcohol) film.