Abstract:The conductive silicon rubber samples were prepared in different filler ingredients; the testing experimental platforms were built and the testing methods were also designed. The body piezoresistive properties, surface piezoresistive properties, relaxation properties of the materials under hydrostatic pressure and the surface properties of the material under air pressure were studied respectively. The results show that under the hydrostatic pressure, the samples of 6% acetylene black/2% nano-SiO2 blends exhibit the best piezoresistive performance; with the addition of nano-modified materials and the increasement of the materials thickness, the relaxation time of the conductive silicone rubber can be reduced. After adding the modified materials, the piezoresistive curves are superior to the case of adding acetylene black alone under air pressure; and with the increasement of the samples thickness, the piezoresistive properties of the material will have a good upgrade.