Abstract:A series of silicon, boron-modified waterborne polyurethanes(WPUs)were synthesized with polyester diol, toluene diisocyanate (TDI), γ-aminopropyltriethoxysilane (KH-550) and boric acid. The structure and performance of waterborne polyurethanes were characterized by FT-IR, laser particle size analyzer, surface contact angle measurement, cone calorimeter and smoke density chamber. The results show that siloxane is successfully introduced into the waterborne polyurethane chain segment; the modified waterborne polyurethane has increasing particle size with similar stability. Compared with ordinary waterborne polyurethane film, the contact angle of the modified waterborne polyurethane increases from 51.0° to 98.8°, indicating a degree of hydrophobicity. The peak heat release rate and total heat release of the modified waterborne polyurethane decrease from 408.6 kW/m2 to 246.3 kW/m2 and from 13.8 MJ/m2 to 7.2 MJ/m2, respectively. The smoke density decreases from 272.0 to 161.3, which indicates good fire-retardant and smoke suppressing performance. The tensile strength is also improved.