Abstract:A sisal pulp/cardanol modified PF (PCF) environmental friction material was prepared using PCF as matrix and sisal pulp as reinforcer. The optimal contents of cardanol and sisal pulp were determined by analysing the molecular weight and thermal properties for PCF and testing mechanical and friction properties for the friction material. Moreover, the worn surfaces of friction materials were observed through SEM. The results indicate that PCF has a high molecular weight and a good heatresistance, and its curing temperature decreases 2 ℃ when cardanol accounting for 5% of phenol. Comparing with pure PF matrix friction material, the impact strength, flexural strength and glass transition temperature for sisal pulp/PCF matrix friction material are enhanced by 11.9%, 7.1% and 10 ℃, respectively, with increasing the sisal pulp content up to 4%. Furthermore, frictional properties for low temperature are improved. SEM micrographs of the worn surfaces show that the furrows are obviously reduced by adding 2% and 4% sisal pulp.