Abstract:With polyester polyol poly adipic acid-1,4-polybutylene terephthalate(PBA) as soft segment, diphenyl-methane-diisocyanate (MDI) and chain extender 1,4-butylene glycol as hard segment, dibutyltin dilaurate and triethylenediamine as catalyst, thermoplastic polyurethane hot melt adhesive was synthesized, which has reasonable molecular weight, high softening point, high adhesive strength and good thermal stability. Through studying on the synthesis process, isocyanate MDI, polyester polyol and chain extender content of thermoplastic polyurethane hot melt adhesive, composition and structure of soft and hard segments, effect of isocyanate index (R) on properties of polyurethane hot melt adhesive were discussed. The results show that with the polyurethane prepolymer synthesis temperature at (70±5) ℃, reaction time about 2 h, the chain extending reaction time about 30 min, aging temperature at 100~110 ℃ for 2~3 h, the value of R 1.02, and the dosage of chain extender 1∶0.7 (mole ratio of polyol/1,4-butanediol), the synthesized polyurethane hot melt has reasonable molecular weight, high softening point, excellent physical properties and adhesive strength properties.