    摘要:

    选用实验室自制的碳包覆纳米铜颗粒(Cu@C)为导热填料,以α,ω-二羟基聚二甲基硅氧烷为基体,采用机械共混法制备了碳包覆纳米铜颗粒/室温硫化(Cu@C/RTV)硅橡胶导热复合材料。通过透射电子显微镜、BET法、热导率测试仪、热重分析仪、万能材料试验机及邵氏硬度计等方法和手段,完成Cu@C纳米颗粒填料的微观形貌分析和比表面积测定,并研究了Cu@C填料在低填充量下(<30%)(质量分数,下同)对于Cu@C/RTV硅橡胶导复合材料热导率、热稳定性及力学性能的影响。结果表明,Cu@C纳米颗粒为球形、包覆型核壳结构,平均粒径在50 nm左右,其比表面积为69.66 m2/g。Cu@C/RTV硅橡胶导热复合材料的热导率随着Cu@C纳米颗粒填充量的增加而增大;填充量为30%时,复合材料的热导率可达2.41 W/mK;加入Cu@C纳米颗粒填料能够将RTV硅橡胶的热分解起始温度提高到422 ℃,并延缓其最终分解温度至625 ℃;随着Cu@C/RTV硅橡胶导热复合材料中Cu@C纳米颗粒填充量的增加,复合材料的拉伸强度和断裂伸长率呈下降趋势,而100%定伸应力和硬度则呈增大趋势。

    Abstract:

    By mechanical blending, the conductive filler, carbon coated copper (Cu@C) nanoparticles prepared in lab, were added into α,ω-dihydroxydimethylpolysiloxa base rubber and then the carbon coated copper (Cu@C) nanoparticles/the room temperature vulcanized (RTV) silicone rubber conductive composites were prepared. The morphology and specific surface area of Cu@C nanoparticles, the effect of Cu@C fillers at low filling content (<30%) on the thermal conductivity, thermal stability and mechanical properties of Cu@C/RTV silicone rubber conductive composites were investigated by transmission electron microscopy (TEM), BET method, thermal conductivity analyzer, thermo gravimetric analyzer (TGA), universal material testing machine and Shore durometer. The results show that Cu@C nanoparticles are nearly spherical in shape and possess good core-shell structure, and most of them are in size of 50 nm. The specific surface area of Cu@C nanoparticles is 69.66 m2/g. With increasing the Cu@C filler content, the thermal conductivity of the composites increases correspondingly and achieves 2.41 W/mK when the filler content reaches 30%. Also, the initial and finish thermal decomposition temperature of Cu@C/RTV silicone rubber raise to 422 ℃ and 625 ℃ respectively with addition of Cu@C nanoparticles. Furthermore, the elongation at break and tensile strength of Cu@C/RTV silicone rubber decrease with the Cu@C filler content increasing, while the stress at 100% strain and hardness are increased.

    参考文献
    相似文献
    引证文献
引用本文

吴其光,张海燕,张琇滨.碳包覆纳米铜颗粒/硫化硅橡胶导热复合材料的制备及性能[J].高分子材料科学与工程,2016,32(1):142-146. Qiguang Wu, Haiyan Zhang, Xiubin Zhang. Preparation and Properties of Carbon Coated Copper/Room Temperature Vulcanized Silicone Rubber Thermal Conductive Composites[J]. Polymer Materials Science & Engineering,2016,32(1):142-146.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2016-01-06
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司