Abstract:The high shrinkage and the low impact strength severely limit the applications of the isotactic polypropylene (iPP). In this paper, the microstructure, shrinkage rate, tensile strength and other properties of composites, which were composed of iPP, short glass fiber (GF), maleic anhydride grafted polypropylene (MPP) or composite toughening agents (CTAs) were studied. The results show that the shrinkage of the composite with 30 portions GF added reduces to 0.168% and 0.191% respectively after 24 h and 48 h at room temperature, which is far lower than the shrinkage of iPP. In system of the PP/GF/MPP/CTAs (mass ratio is 55/30/5/10), the tensile strength increases to 61.37 MPa, which is 81.2% higher than that of pure iPP; the tensile modulus is 1545 MPa, which is 118% higher than that of iPP; the impact strength is 20.11 kJ/m2, which is 225% higher than that of iPP.