Abstract:The blends of poly (lactic acid) (PLLA) and poly (3-hydroxybutyrate-co-4-hydroxybutyrate) (P34HB) with 4-hydroxybutyrate (4HB) molar fraction of 11% and 17% were prepared via melt blending. In order to study the effect of 4HB content of P34HB on the miscibility, melting behaviors and mechanical properties of the blends, scanning electronic microscope (SEM), dynamic mechanical analysis (DMA), differential scanning calorimetry (DSC) and mechanical test were used. The results show that the two glass-transition temperatures (Tg) of PLLA/P34HB blends get close to each other, meaning that PLLA/P34HB blend is partially miscible at the content of P34HB higher than 25%. Besides, the more 4HB content, the better miscibility of PLLA/P34HB. The crystallization ability of PLLA for PLLA/P34HB decreases with increasing P34HB content, and the crystallization ability of PLLA for PLLA/P34HB with molar fraction 17% 4HB is greater than the one with 11% 4HB due to the inferior miscibility of the former. The tensile strength of PLLA/P34HB blends reduces and the elongation at break of PLLA/P34HB blends improves with increasing content of P34HB. Meanwhile, the mechanical properties of PLLA/P34HB are lower for the blends with higher 4HB content because of the poorer miscibility.