Abstract:A kind of comb like polymer light stabilizer (P(HAPBT-co-MTMP-co-OA-co-mPEGA) was synthesized by solution copolymerization. The structure of copolymers was confirmed by FT-IR, 1H-NMR and TGA. The results show that the thermal decomposition temperature of the polymer light stabilizer is significantly higher than the decomposition temperature of the intermediate(2′, 4′-dihydroxy-phenyl)-2H-benzotriazole. Then the polymer light stabilizer was applied to the polypropylene/sisal fiber(PP/SF) and polyethylene(PE)/SF composite materials to improve the UV aging resistance of the materials. The UV aging properties of SF/PP and SF/PE Wood plastic composites were studied by tensile strength retention rate, contact angle of material surface, carbonyl index, vinyl index, loss rate of water extraction and loss rate of heat extraction before and after aging. The microstructure of the composite was observed by SEM, and the light stability properties of the polymer light stabilizer and UV-P were compared. The results show that the tensile strength retention rates of the PP/SF and PE/SF composites with addition of the polymer light stabilizer are decreased by 37.41% and 38.17% respectively less than that of the blank composites after 50 d of UV light aging. While the tensile strength retention rates of the PP/SF and PE/SF composites with the UVP light stabilizer are decreased by 12.72% and 12.85% respectively less than that of the blank composites. The vinyl index of PP/SF and PE/SF composites with polymer light stability increases by 0.033 and 0.018 respectively, the carbonyl index increases by 0.07 and 0.039 respectively, but the increasing range is very narrow. The results of contact angle test show that the contact angle of PP/SF and PE/SF decrease with the increase of UV aging degree, regardless of whether the light stabilizer is added or not, but the contact angle of the composite with light stabilizer is significantly lower than that of the blank. SEM show that with the addition of light stabilizers for polymer composites after aging, exposed sisal fiber surface area is relatively small, fewer cracks. The polymer light stabilizer has better hot water extraction resistance and heat transfer resistance performances than the UV-P.