Abstract:Polylactide stereocomplex (sc-PLA) and flax/sc-PLA composite were prepared by melt blending and then followed by injection molding. The effects of the reinforcement of flax fiber and the interfacial modification of hexamethylene diisocyanate (HMDI) on the structure and properties of flax/sc-PLA composite were investigated by DSC, DMA, TGA, SEM, Vicat softening temperature test and mechanical property test, respectively. It is found that the degree of stereocomplex crystallization, thermal resistance and tensile strength are improved obviously with the addition of flax fiber. The degree of stereocomplex crystallization of flax/sc-PLA composite is increased from 17.3% to 24.9%. The Vicat softening temperature of composite is improved from 161.1 ℃ to 195.7 ℃, and the tensile strength of composite is enhanced from 57.4 MPa to 62.5 MPa. Moreover, the interfacial compatibility of flax/sc-PLA composite is improved by the interfacial modification of HMDI, and the tensile strength of flax/sc-PLA composite is further increased to 70.4 MPa. In addition, the thermal stability of flax/sc-PLA composite is also increased by the modification of HMDI. The onset degradation temperature and storage modulus G′ of flax/sc-PLA composite are improved significantly than unmodified composite.