Abstract:Based on ring opening copolymerization of L-lactide (L-LA) and polyethylene glycol 400 (PEG-400), secondary polymerization was carried out using L-lysine with biocompatibility to prepare L-lysine modified poly(lactic acid)/poly(ethylene glycol) copolymers. Obvious differences of PLLA, PLLA-PEG copolymer and L-lysine modified PLLA-PEG copolymer were characterized by FT-IR, NMR, XRD, DSC, GPC and contact angle measurement analysis (CA). The experimental results show that ΔH and Tm of L-lysine modified PLLA-PEG copolymer synthesized fall from 81.57 J/g and 177.34 ℃ of pure PLLA to 46.02 J/g and 151.34 ℃ respectively, which effectively improve the chain flexibility and crystallinity. In addition, number-average molecular weight (Mn) of the copolymer decreases gradually from by 7.7×104 of pure PLLA to 3.2×104, and its dispersivity (Mw/Mn) becomes wider, but the increase of CA makes the hydrophilic higher, which could expect to be applied in the field of tissue engineering.