Abstract:To improve the sphericity and wall thickness uniformity of thick-walled polymer shells used for laser inertial confinement fusion, poly(acrylic acid) (PAA) was added in the external phase (W2). The effects of PAAs with different molecular weights and poly(vinyl alcohol) (PVA) on deformation of the PS compound droplets were investigated. The experimental results show that PS compound droplets with 900 μm diameter prepared with PVA are stable due to the hydrophilic and hydrophobic groups, but these groups signifcantly reduce the interfacial tension, the Laplace pressure decreases with increasing the diameter, leading to the deformation increase and PS compound droplets with 1900 μm diameter breaking up, forming PS droplets without the inner water (W1). The interfacial tension of PAA with lower molecular weight (L-PAA) solution is much higher than that of the PVA solution, but their viscosities are almost the same, so the drag force for forming the droplet is much lower than that force for preventing it from being separated from the tube tip, resluting in that the formation of the droplets is difficult. Moreover, two or more PS compound droplets prepared with L-PAA coalesce to form bigger droplets in a short time after the generation, probably due to relative shorter chain. PS compound droplets with both 900 μm and 1900 μm diameter prepared with PAA with higher molecular weight (H-PAA) are stable, probably due to the steric stabilization of their longer chains. Moreover, compared with PVA system, H-PAA improves the sphericity of these PS shells, due to the higher interfacial tension.