Abstract:The target product epoxidized diisooctyl methyl-α-eleostearate maleate (EDOMEM) was obtained and then blended with dioctyl-phthalate (DOP) used as complex plasticizer to plasticize poly (vinyl chloride) (PVC). And EDOMEM was characterized by FT-IR. TGA, TGA-FT-IR, TGA-MS, torque rheometer and the mechanical properities were used for evaluating the PVC blends. The results indicate that the initial thermal degradation temperature (Ti), the 10% mass loss temperature (T10) and the 50% mass loss temperature (T50) respectively increase 5.6 ℃, 12.6 ℃ and 25.4 ℃ compared with F0. TGA-FT-IR and TGA-MS detect that the main pyrolysis products of PVC blends are H2O, CO, HCl, CO2 and C6H6. When the EDOMEM content increases from 0% to 33.3% (the total quality of plasticizer), the elongation at break raises 9%, improving flexibility of the PVC blends. The dynamic stability time is prolonged from 12.11 min to 40.24 min. Moreover, the loss of voalitity and extraction decrease with the content of EDOMEM increasing. Therefore, EDOMEM can be used as secondary plasiticizer for PVC.