Abstract:Micro-filtration membrane of chloromethylated polysulfone (CMPSF) was first prepared by phase inversion method, and then CMPSF membrane was chemically modified with ethidene diamine. A surface-initiated system -NH2/S2O82- was constituted by using the primary amino group on the membrane surface and the ammonium persulfate in the aqueous solution, and the tertiary amine monomer N,N-dimethylaminoethyl methacrylate(DMAEMA) was made to produce graft-polymerization, resulting in the porous grafted membrane PSF-g-PDMAEMA. The effects of the main factors on the graft-polymerization were examined, and the grafted membrane was fully characterized. The adsorption abilities of the grafted membrane for two toxic anions, chromate and molybdate, were examined, and the membrane separation and removal behavior of the grafted membrane for CrO42- ion was studied. The experimental results show that the grafted membrane PSF-g-PDMAEMA with a grafted degree of 0.64 mg/cm2 of PDMAEMA can be obtained by controlling the concentration of ammonium persulfate as 1% and the reaction temperature at 50 ℃. In acidic and neutral solution, by right of the strong electrostatic interaction, the grafted membrane PSF-g-PDMAEMA has strong adsorption ability for CrO42- and MoO42- anions. As the membrane separation process is carried out by using the grafted membrane PSF-g-PDMAEMA as filter membrane, CrO42- ion in water can be effectively removed by selective adsorption.