Abstract:By simple chemical oxidation polymerization method, cross-linked polyaniline (PANI) networks were successfully prepared, and the composite of PANI and multi-walled carbon nanotube (MWCNT) was also obtained by in-situ polymerization, in which camphorsulfonic acid, ammonium persulfate and dioctyl-sulfosuccinate sodium salt were used as doping acid, initiator and surfactant, respectively. The morphology analysis results indicate that cross-linked PANI is successfully wrapped on MWCNT surfaces. PANI/MWCNT composite exhibits the specific capacitance of 639.7 F/g at a current density of 0.5 A/g, showing a significant improvement in capacitance as compared to pure PANI (498.7 F/g). PANI/MWCNT composite delivers 77.2% retention of initial capacitance at a current density of 5.0 A/g after 1000 charge-discharge cycles, whereas pure PANI only retains 65.1%, indicating that the addition of MWCNT can enhance the electrochemical stability of PANI.