Abstract:The silica surface was modified with three different silane coupling agents (Si69,KH570,11-100),and modified-SiO2/natural rubber (NR) composite materials were prepared. The structure and property of modified-SiO2 and modified-SiO2/NR composite materials were characterized by FT-IR,TG,SEM,and rubber process analyzer (RPA). The mechanical and sulfuration property of natural rubber composite materials were studied. The results show that three silane coupling agents is successfully grafted onto silica surface and for modified-SiO2/NR compared with unmodified-SiO2/NR, the scorch time becomes longer, the cure time is shortened,bound and the rubber content increases. In addition, the stress at definite elongation and the tear strength distinctly increase, but the elongation at break decreases; at the same time, the dispersion of modified silica in the natural rubber matrix improves significantly, the dispersion of Si69-SiO2 is the best; Si69-SiO2/NR has the lowest rolling resistance and calorigenesis. Besides, the roughness of stretching surface of fracture of modified-SiO2/NR composite material increases.