    摘要:

    以聚四氢呋喃醚二醇(PTMG)为软段,甲苯二异氰酸酯(TDI)、二苯基甲烷二异氰酸酯(MDI)、混合异氰酸酯(n(TDI)∶n(MDI)=1∶1)分别为硬段,采用预聚体法合成了一系列不同硬段微区结构的聚氨酯脲弹性体,并通过红外光谱、热重分析、差示扫描量热以及力学表征等方法,研究了不同硬段微区结构与聚氨酯脲(PUU)体系内部微相分离、热稳定性及力学性能的相关性。结果表明,TDI型聚氨酯脲的NH 官能团伸缩振动谱带出现在较低位置(3270cm-1),MDI型NH 官能团伸缩振动谱带出现在相对较高的位置(3285cm-1),前者的Tg(-57.6℃)低于后者Tg(-49.5℃),而初始降解温度前者(294℃)高于后者(268℃),混合型的均位于两者之间。因此,TDI型PUU 表现出较高的微相分离程度和硬段微区有序度,而MDI型微相混合程度较高、且微相混合程度有助于力学性能的改善。随着温度的升高,PUU内部氢键化NH 官能团伸缩振动吸收强度逐渐减弱,谱带吸收位置由低波数向高波数移动,力学性能逐渐下降,当温度处于70℃左右时,其波数出现轻微的突越,力学性能也表现出较快的下降趋势。

    Abstract:

    A series of polyurethane urea (PUU) elastomers were prepared, based on polytetramethyleneether glycol(PTMG) used as soft segment, tolylene diisocyanate(TDI), diphenyl methane diisocyanate(MDI) and mixture of TDI/MDI for their mole ratio of 1∶1 as hard segment. The mechanical properties and heat resistance of PUU were investigated through correlation among the structure of hard segment micro-phase. The results show that the NH group stretching vibration band of TDI-based appears at 3270 cm-1, and that of MDI-based appeares at the higher wave number (3285 cm-1). Additionally, Tg (-57.6 ℃) of TDI-based(-57.6 ℃) is lower than that of the MDI-based (-49.5 ℃), and the initial degradation temperature instead. Mixture-based is located between them. Compared with MDI-based, the TDI-based shows the higher micro-phase separation degree, but exhibits worse mechanical properties. And with the temperature increasing, the absorption intensity of hydrogen bonded NH stretching vibration band is gradually weakened, and the band site shifts from the lower wave number to the higher wave numbers, and the mechanical properties of the PUU decrease gradually. When the temperature is 70 ℃, the slightly jump of wave numbers is observed , and the mechanical properties drop quickly.

    参考文献
    相似文献
    引证文献
引用本文

赵洪祥,蒋玉湘,赵天宝,罗明艳,周京福,李再峰.硬段微区结构与聚氨酯脲弹性体力学性能及耐热性的相关性[J].高分子材料科学与工程,2017,33(6):100-104. Hongxiang Zhao, Yuxiang Jiang, Tianbao Zhao, Mingyan Luo, Jingfu Zhou, Zaifeng Li. Correlation Among the Structure of Hard Segment Micro-Phase, Mechanical Properties and Heat Resistance for PUU Elastomers[J]. Polymer Materials Science & Engineering,2017,33(6):100-104.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2017-06-21
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司