Polyurethane-poly(ethyl acrylate) (PU/PEA) hybrid emulsions and polyurethane- poly(butyl acrylate) (PU/PBA) mixed emulsion flexible were synthesized by seed emulsion polymerization and physical blending crosslinking. The emulsion is not only environmentally friendly, but also has high strength, good elasticity and excellent adhesion. The results of drag tests show that the PU/PEA (40/60) hybrid emulsion coating has certain drag reduction effect, the drag rate is high when the flow velocity is high, and the average drag reduction ratio reaches 5% at the flow velocity of 0.5~3 m/s, especially the drag reduction rate is 8% when the flow rate is 3.0 m/s. The particle image velocity test gived the comparison of the average frictional resistance coefficient of the flexible wall with the aluminum plate under the same Reynolds number, and the calculated drag reduction rate. The results show that the effect of PBA / PU and P (BA-EA) / PU is about 5.3%, while the average reduction of PBA / PU-MMA is not drag reduction. The PBA/PU-MMA shows drag reduction at low-speed, and non-drag reduction at high-speed. The PU/PBA mixed emulsion coatings also have certain drag reduction effects and the drag reduction ratio is 7% or 4% at 0.5 m/s or 1 m/s of the flow velocity, respectively.