Abstract:Styrene-isoprene-butadiene terpolymer(SIBR)was synthesized with n-BuLi as initiator,2,2-bis[(5-methyl-2-oxolanyl)]propane(DMOP) as polar modifier by anionic polymerization. The effects of n(DMOP)/n(n-BuLi)and polymerization temperature on copolymerization kinetics were investigated,the microstructures of SIBR were analyzed, and the comparison was conducted with system of tetrahydrofuran(THF)as polar modifier. The results show that under the conditions of mass fraction of monomer is 12%,mass ratio of St/Ip/Bd is 22/38/40,relative molecular weight is 12×104,the polymerization rate of St, Ip and Bd is linear with monomer concentration,the polymerization rate of St, Ip and Bd and the apparent propagation reaction rate constants (Kp″) increase gradually with the increase of mole ratio of DTHFP/Li and the rise of polymerization temperature. When the mole ratio of DMOP/Li is 1.0,the apparent chain propagation activation energies of St, Ip and Bd is 71.868 kJ/mol, 53.553 kJ/mol, 71.403 kJ/mol, respectively. The freauency factors of St, Ip and Bd is 6.61×1010 min-1,5.68×107 min-1,7.88×1010 min-1, respectively. With the increase of mole ratio of DMOP to n-butyl lithium or the decrease of polymerization temperature,the content of total 1,2-structure and Ip3,4 increases dramatically,the content of Bd1,4 and Ip1,4 decreases clearly. When using a small amount of DMOP,the effect is better than that of using a large amount of THF,the ability of improving the polymerization rate of DMOP is much more effective than that of THF.