Abstract:In this paper, the decomposition process of paraffin waxes, conformal polymers (mixtures of PP and HDPE), paraffin / conformal polymerization (PP/HDPE) and tungsten carbide (WC-10%Ni) Ni powder injection molding feedstock was analyzed by thermogravimetric methodin nitrogen at four different heating rates (5 ℃/min, 10 ℃/min, 15 ℃/min and 20 ℃/min). The thermal decomposition kinetics of these four materials was analyzed by Kissinger method and Flynn-Wall-OZAWA method, and the reaction order was studied by Coats-Redfernformulation. The results show that the Kissinger method does not reflect the complex pyrolysis process of the mixture welland can not support the one-step thermal debinding process of tungstencarbide powder for feedstock injection molding. Determined by Flynn-Wall-OZAWA method, the pyrolysis activation energy of paraffin wax, conformal polymer, paraffin/conformal polymer and tungsten carbide (WC-10%Ni) nickel powder injection molding feedstock is respectively 59~72 kJ/mol, 143~252 kJ/mol, 60~240 kJ/mol and 93~220 kJ /mol respectively. The pyrolysis of paraffin and conformal polymers can be described by the first order reaction,while the mixture of paraffin/conformal polymer and WC-10%Ni is described by three successive first-order reactions.