    摘要:

    研究了次氯酸钠(NaClO)对废旧橡胶颗粒(GTR)的表面改性,得到了表面氧化和氯化的改性GTR颗粒(mGTR),并制备了废旧橡胶颗粒/聚氨酯(GTR/PU)复合材料。通过X 射线光电子能谱、扫描电镜、接触角等手段对GTR 进行了表征,研究了NaClO 溶液在不同处理时间对GTR表面改性效果的影响。结果表明,通过NaClO 溶液改性后,GTR表面的极性官能团数量增加、粗糙度增加、润湿性提高,最佳处理时间为10min。改性后的GTR制备的复合材料力学性能及与钢板的粘接性能明显提高,与未改性GTR相比,10min处理的GTR制备的复合材料拉伸强度提高36%,粘接强度提高127%。

    Abstract:

    In this paper, the ground tire rubber (GTR) was surface modified with NaClO solution, and the GTR/PU composites were fabricated. The GTR was characterized by XPS, SEM and contact angle tests to investigate the modification effect at different treatment time. The results show that the number of polar functional groups on the surface of GTR is increased, the roughness is increased, and the wettability is improved after modification, the optimum treatment time is 10 min. Meanwhile, the mechanical properties and the adhesion properties of the composites prepared by the modified GTR are significantly improved. Compared with the unmodified GTR,when the treatment time of GTR is 10min, the tensile strength of the GTR/PU composites is increased by 36%, while the adhesive strength to steel plate is increased by 127%.

    参考文献
    相似文献
    引证文献
引用本文

尚文翰,李 姜.废旧橡胶颗粒的表面改性及粘接性能[J].高分子材料科学与工程,2018,34(10):99-104. Wenhan Shang, Jiang Li. Surface Modification of Ground Tire Rubber and Its Adhesion Property[J]. Polymer Materials Science & Engineering,2018,34(10):99-104.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2018-11-08
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司