Abstract:The 7 mm polymethylmethacrylate(PMMA)-polycarbonate(PC) composite boards were molded by compression injection and quantitative measured by photoelastic method to analyze the effect of parameters on residual stress based on photoelastic method. The 3mm PMMA board was firstly made by normal injection molding and then was put in 7 mm mold cavity. After that, 7 mm PMMA-PC composite board was prepared by compression injection molding. The processing parameters like packing pressure, packing time, melt temperature, mold temperature and compression stoke were studied. The results show that, with the increase of packing pressure or packing time, the curves of stress vary likes parabola; the increase of the melt temperature and compression distance will reduce the residual stress of the composite board. The rising mold temperature increases the residual stress of the composite board, because the asymmetric cooling increases the thermal residual stress of composite plate. When the mold temperature is 70 ℃ or 80 ℃, the composite board residual stress is smaller and uniformly distributed. Compared to all of process parameters, mold temperature and melt temperature have the most significant effect on the residual stress of the composite board.