Abstract:Full biobased benzoxazine monomers containing flexible long chain (CFa and UFa) were synthesized using cardanol, urushiol, furfuryl amine and paraformaldehyde as raw materials. Then, the flexible polybenzoxazine films (PCFa and PUFa) were obtained by thermally curing. The chemical structures of CFa and UFa were characterized by FT-IR and 1H-NMR. At the same time, the thermal curing behavior, ability of forming film of monomers and thermal, dynamic mechanical and water absorption properties of the corresponding polybenzoxazines were compared. Results of FT-IR and DSC show that the ring opening polymerization occurs at high temperature. The temperature of ring opening polymerization of UFa is lower than that of CFa. By DMA analysis, the glass transition temperatures of PCFa and PUFa are 85 ℃ and 143 ℃, and the storage modulus is 203.2 MPa and 510.7 MPa, respectively. The 5% mass loss temperature is 372 ℃ and 395 ℃, respectively. In different pH environment, the water absorption ratio of PUFa is lower than that of PCFa.