Abstract:A fluorenyl diamine monomer with hydroxyl and ether linkage 9,9’-bis[4-(4-amino-2-hydroxybenzoxyl) phenyl] fluorene was synthesized. Five kinds of polyimides (PI) were prepared from the diamine with 4,4'-(Hexafluoroisopropylidene)diphthalic anhydride (6FDA), pyromellitic dianhydride (PMDA),3,3',4,4'-biphenyltetracarboxylic dianhydride (BPDA),3,3',4,4'-benzophenonetetracarboxylic dianhydride(BTDA)and 4,4'-oxydiphthalic anhydride (ODPA) via the thermal imidization of poly( amic acid) respectively.The structure and properties of the diamine and PI were characterized by TGA, FT-IR, XRD, NMR, UV-vis, DSC, and solubility test. The results show that the fluorenyl Cardo polyimides containing hydroxyl exhibit amorphous structure. Most PI show good solubility in organic solvents such as DMF, DMAc, NMP and DMSO. PI-6FDA show the best thermal properties,10% thermal decomposition temperature is 443 ℃ and the glass transition temperature (Tg) of PI-6FDA, PI-PMDA and PI-BPDA is 343 ℃, 346 ℃ and 345 ℃ respectively.PI-ODPA has the best mechanical property because of ether linkage can improve the flexibility of molecular chains.