Abstract:CaCl2/formid acid (FA) system was adopted to dissolve degummed silk, the effects of solution preparation conditions (one-step, two-step) on the fiber formation and fiber properties were discussed. The results indicate that these two methods could obtain the silk fibroin solutions which characterized by preserving the natural fibril structure, however, the fibril size in the spinning solution is different. In the one-step method, the salt in the spinning solution is not removed and the fibrils are longer, so the formation of fibers is affected. The diameter of nanofibers is uneven, and the fibers are easy to adhesion. The diameter of the fibril in the solution prepared by the two-step method is similar to that by the one-step method, but the length is reduced to (90~140) nm, the spinnability of the fiber is improved, the surface of the fiber is smoother, the fineness is more uniform, and the draftability of the fiber is enhanced. After 0.5 times of drawing, the stress at break increases to (16.5±1.5) MPa, the elongation at break reaches 17.2%±2.4%, and the degradation rate after 30 d of degradation is only 5.2%.