Abstract:Film formation property of natural rubber latex is an important process property of latex, which directly affects the quality of products. Film formation properties of latex are known to be influenced by the content of proteins and phospholipids. In this paper, the deproteinized natural rubber (DPNR), lipid-free natural rubber (PNR) and lipid-free DPNR (P-DPNR) were prepared by high speed refrigerated centrifugation, treated with enzyme decomposition (alkaline proteinase, lipid enzyme) and high speed centrifugation, research on the impact of proteins and phospholipids to the particle size, molecular weight, drying properties, and surface morphology was applied, and the film formation mechanism was analyzed. The results show that nitrogen content and lipid content decreases; the average particle size becomes larger; the average molecular weight of DPNR and PNR decreases by 1.33×105, 1.34×105, the molecular weight distribution becomes wider; the drying rate of film increases; the surface morphology of the film tends to be flat, the roughness of film decreases. The influence of protein and phospholipid on the film formation process of latex was analyzed, and the mechanism of film formation process was proposed. The film formation process can be divided into four stages: water evaporation, particle deforming, coalescence, and inter-diffusion.