Abstract:The SA-Al2O3/TPU composites were prepared by the slab casting method using polyurethane elastomer (TPU) as matrix and stearic acid (SA) modified alumina as filler. The chemical structure of SA-Al2O3 was characterized by FT-IR, the crystallinity of the SA-Al2O3 and composites was analyzed by XRD. Meanwhile, the morphology, mechanical properties, thermal stability and corrosion resistance of SA-Al2O3/TPU composites were observed by SEM, tensile test, TG and brine immersion experiment, respectively. The results show that the chemical structure and the crystal form of Al2O3 modified with stearic acid do not change, the contact angle increases to 160.8°. Satisfying a certain range of usage, the content of added SA-Al2O3 in the composite materials reaches 40%, the tensile strength and the elongation at break are 20.74 MPa, 446.55% respectively, the thermal stability and the corrosion resistance are better.