Abstract:Solid-state shear milling (S3M) technology was used to prepare polyoxymethylene/polyethylene oxide/molybdenum disulfide (POM/PEO/MoS2) co-powders and composites. Then, scanning electronic microscope (SEM), universal material testing machine, thermogravimetric analyzer (TGA) and friction wear tester were further used to investigate the corresponding morphology, particle size distribution, mechanical performance, thermal stability and friction and wear properties. The experimental results show that, under effect of the strong three dimensional shear force field during pan-milling, the PEO modifier and MoS2 filler particles are uniformly dispersed in the POM matrix and the size of the co-powder decreases to the micrometer level. The co-effect of the introduced PEO modifier and pan-milling could effectively improve the impact property of POM. In the meantime, the encapsulation of MoS2 particles with PEO also effectively solves the problems of the low thermal stability and degradation of POM during processing. In addition, the combination of PEO and MoS2 could significantly reduce the friction coefficient and wear volume of POM, endowing the obtained POM/PEO/MoS2 ternary composite with excellent self-lubrication and friction performance.