Abstract:A heat-resistant composite of ethylene-propylene-diene monomer rubber (EPDM) was prepared. Dicumyl peroxide (DCP) was used as main crosslinking agent. Effects of N-isopropyl-N′-phenyl-p-phenylenediamine (4010NA) and 2,2,4-trimethyl -1,2-dihydroquinoline (RD) on EPDM composites were investigated. Mooney viscosity, vulcanization curve, tensile strength, TGA , hot-air-aging strength and FT-IR were used to characterize the process, mechanics, thermal cracking, thermo-oxidative-aging properties of composites. The results show that with the increasing content of antioxidant from 0 phr to 8 phr, the fluidity decreases with 4010NA while changing little with RD. The tensile strength decreases with 4010NA and RD, while the same content of 4010NA decreases the intensity more obviously. Appropriate 4010NA and RD improve the thermal-oxygen-aging strength of EPDM significantly, while 4010NA-based EPDM is slightly lower at both high-temperature-cracking and thermal-oxygen-aging properties of 150 ℃× 168 h than RD-based EPDM. Through FT-IR, the stretching vibration peak of N-O appears at 1309 cm-1 in the heat-treated 4010NA/DCP, and it can be concluded that the mechanism of improving the thermal-aging performance is that the N-O-C groups can capture oxygen and generate free radicals for crosslinking EPDM.