Abstract:A fully phenylacetylene end-capped silicon-containing arylacetylene resin (FEC-PSA) and a propargyloxy-containing benzoxazine (P-appe) were synthesized and used to blend with silicon-containing arylacetylene resin (PSA) to prepare four kinds of modified silicon-containing arylacetylene resins by physical mixing. The unidirectional T800 carbon fiber reinforced modified PSA resin composites were prepared by hot press molding. The structure and properties of modified PSA resins and composites were studied by FT-IR, 1H-NMR, DSC, TGA and so on. The results show that the viscosity of the blended PSA resins decreases markedly with increasing temperature as well as increasing mass fraction of P-appe in the blended resins. The temperature at 5% mass loss (Td5) and residual yield at 800 ℃ of the cured blended resin (PFP-3) with 30% mass fraction of P-appe are 531 ℃ and 85%, respectively. The flexural strength and impact strength of the cured PFP-3 resin are 41.5 MPa and 5.5 kJ/m2, respectively. The flexural strength, flexural modulus and interlayer shear strength of the unidirectional T800 carbon fiber reinforced PFP-3 composite are 1557 MPa, 153 GPa and 66 MPa at room temperature, respectively.