聚乳酸及其共聚物单丝的体外降解性能
作者:
作者单位:

作者简介:

通讯作者:

中图分类号:

基金项目:

先进金属电力材料重点实验室(17ZR1419600);上海市科学技术委员会(11441900501)


Vitro Degradation Properties of Poly (L-lactide) and Its Copolymer Monofilaments
Author:
Affiliation:

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    通过熔融挤出-热拉伸分别制备了PLLA、PLCL 95/5和PLGC 89/8/3单丝。经环氧乙烷灭菌处理后的3种单丝置于37 ℃的磷酸盐缓冲溶液(pH=7.4±0.2)中进行180 d的体外降解。采用失重率分析、扫描电镜、凝胶渗透色谱分析、差示扫描量热分析、X射线衍射及力学性能测试等方法分别对3种单丝的降解性能进行了研究。结果表明,丙交酯单体含量对PLLA及其共聚物的降解性能有较大的影响。PLLA单丝经过180 d的体外降解,单丝的表面形态和失重率几乎不变,力学性能缓慢降低;对于PLCL 95/5单丝,在降解前60 d,相对分子质量和熔点(Tm)明显下降,力学性能基本丧失;而PLGC 89/8/3单丝降解最快,在降解前30 d,相对分子质量和Tm显著降低,力学性能完全消失。根据降解的一级动力学模型计算出PLCL 95/5单丝降解速率比PLLA单丝快5.0倍,PLGC 89/8/3单丝的降解速率比PLLA快8.0倍。

    Abstract:

    PLLA, PLCL 95/5 and PLGC 89/8/3 monofilaments were prepared by melt-extrusion and tensile orientation. Then the three kinds of monofilaments were incubated in phosphate buffer media (pH=7.4±0.2) at 37 ℃ for 180 d. Furthermore, the degradation properties of the three kinds of monofilaments were investigated by mass loss ratio, SEM, GPC, DSC, XRD and mechanical properties testing. Degradation results show that the proportion of L-lactide has a great influence on the degradation properties of PLLA and its copolymer. After 180 d of in vitro degradation, the surface morphology and mass loss ratio of PLLA monofilaments exhibit no significant changes, except the breaking strength and breaking elongation decrease slowly. For PLCL 95/5 monofilament, its molecular weight and Tm decrease significantly after 120 d degradation, leading to almost total loss of mechanical properties; obviously, PLGC 89/8/3 monofilament degradation is the fastest, just within only 30 d degradation, its molecular weight and Tm are decreased sharply, the mechanical properties completely disappear. According to the first-order kinetic model, the PLCL 95/5 monofilament is degraded 5.0 times faster than PLLA, and the PLGC 89/8/3 monofilament is degraded 8.0 times faster than PLLA.

    参考文献
    相似文献
    引证文献
引用本文

杨彩红,马凤仓,高晨光,康亚红,张国艺,姜洪焱.聚乳酸及其共聚物单丝的体外降解性能[J].高分子材料科学与工程,2019,35(11):101-108. Caihong Yang, Fengcang Ma, Chenguang Gao, Yahong Kang, Guoyi Zhang, Hongyan Jiang. Vitro Degradation Properties of Poly (L-lactide) and Its Copolymer Monofilaments[J]. Polymer Materials Science & Engineering,2019,35(11):101-108.

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:
  • 录用日期:
  • 网络出版日期:
  • 在线发布日期: 2019-12-23
  • 出版日期:
您是第      位访问者
编辑出版 :《高分子材料科学与工程》编辑部
地址 :四川省成都市一环路南一段24号 四川大学高分子研究所
电话 :028-8540 1653  E-mail:gfzclbjb@vip.sina.com
高分子材料科学与工程 ® 2026 版权所有
技术支持:北京勤云科技发展有限公司